Please use this identifier to cite or link to this item:
https://elib.belstu.by/handle/123456789/14693
Title: | Filled paper pulp sizing features in the presence of polyelectrolyte |
Authors: | Shcherbakova, T. O. Chernaya, N. V. Chubis, P. A. Zholnerovich, N. V. Savanovich, O. Yu. |
Keywords: | бумажная масса свойства бумаги технология бумаги наполнители склеивание бумаги |
Issue Date: | 2014 |
Publisher: | BSTU |
Citation: | Filled paper pulp sizing features in the presence of polyelectrolyte / T. O. Shcherbakova [et al.] // Proceedings of BSTU. No. 4. – Minsk : BSTU, 2014. – P. 108-111 |
Abstract: | It is shown that to reduce the size of the filler particles from 3–5 microns (natural) to 0.65–0.82 microns ({[CaCO3]m· nCO3 2– · (n – x)Na + } x– · xNa + ) allows for the filling process in geteroadagulation and penetration. To obtain high elevated paper with high-hydrophobic and strength properties it is advisable to sequentially introduced into the pulp slurry, calcium chloride and sodium carbonate to obtain superfine particles of filler (consumption10% of a. d. f.), then polyethylenimine (consumption 0.075% a. d. f.) and adhesive based on alkylketenedimer AKD (consumption 0.5% a. d. f.) demonstrating flocculating and sizing effect respectively. |